Waste-to-energy furnace anticorrosion selection.

SEP 06, 2026 · TECH & INDUSTRY

Waste-To-Energy Furnace: High-Temp + Acid Erosion Dual Attack — How to Select Coatings?

Waste incineration furnace water wall and superheater

Waste-to-energy furnaces expose water walls and superheaters to 450–650 °C together with acidic condensation from flue gas, causing rapid tube thinning and unplanned outages.

High-temperature zone

JIANBANG JB-800 ultra-high-temperature coating serves up to 1200 °C on water walls and superheaters, resisting oxidation and thermal shock.

Flue-gas side

JB-015 flue-gas lining coating protects ductwork, economizers and desulfurization sections from acidic condensation and abrasion.

Related Products
JB-800 (≤1200°C) · JB-015 (flue-gas lining, acid condensation)
Recommended keywords: waste-to-energy · incineration anticorrosion · high temperature coating · JB-800 · JB-015